| Type |
Acid Value( mgKOH/g) |
viscosity(pa·s/200°C) |
Glass Transition Temp(Tg℃) |
Curing Time(℃/min) |
Properties |
| FH9868 |
50~60 |
3.0~8.0 |
64~68 |
200°C×15′ |
For two-component ,transfer and low gloss powder with FH9828. |
| FH9878 |
48~58 |
5.0~9.0 |
66~68 |
200°C×12′ |
Boiling resistance、Wood grain transfer,For two-component low gloss powder |
| FH9928 |
17~23 |
2.0~5.0 |
56~58 |
200°C×12′ |
For two-component Super weatherability with FH9968 |
| FH9968 |
58~68 |
2.0~5.0 |
64~66 |
200°C×12′ |
Boiling resistance、For two-component Super weatherability with FH9928 |
| FH9833 |
48~55 |
3.0~6.0 |
63~65 |
200°C×15′ |
For two-component , low gloss powder with FH9813 or FH9818.Economical type. |